MoCu Alloy

MoCu, Molybdenum and Copper, has high thermal conductivity, a low thermal expansion coefficient, is non-magnetic, has good machinability, and performs well in high temperatures.

The following datasheet gives an overview of MoCu Alloy.

Chemical Composition

Element Content(%)
Molybdenum (Mo) 40-85%
Copper (Cu) 15-60%

Physical Properties

Properties Metric Imperial
Density 9.42-10 g/cm³ lb./in³

Mechanical Properties

Properties Metric Imperial
Tensile Strength 230-380 MPa psi
Yield Strength (@ proof 0.200%) MPa psi
Elastic Modulus GPa ksi
Poisson’s Ratio
Elongation at Break
Hardness, Rockwell B
Hardness, Brinell

Thermal Properties

Properties Metric Imperial
Thermal Expansion co-efficient (@ 100 – 538°C/212 – 1000.4°F) µm/m°-C µin/in°F
Thermal Conductivity (@ 21°C/70.0°F) W/mK BTU in/hr.ft².°F

Applications

CMoCu is used in the following applications:

AS9100 / ISO9001:2015 Accreditation Logo

Quality Policy: Vulcan Metal Group, LLC. supplies mission critical, special purpose materials, and products at a competitive price. The company’s quality system is registered to ISO 9001 and AS9100 and follows its principles for the governance of the business. An active continual improvement program and compliance with all applicable OSHA, federal, and state regulations is maintained.